Saltar al contenido

← Todos los procesos

PTA and PET chain

Petrochemical process

Paraxylene is oxidised to purified terephthalic acid (PTA), which is reacted with mono-ethylene glycol to make PET for bottles, film and polyester fibre.

Carga
Paraxylene, air, acetic acid, mono-ethylene glycol
Produce
Purified terephthalic acid (PTA), PET resin (bottle grade), Polyester fibre and film
Catalizador
Cobalt, manganese and bromide in acetic acid (oxidation)

Flujo del proceso

Qué hace

In the Amoco process, paraxylene is oxidised with compressed air in acetic acid solvent, using a cobalt, manganese and bromide catalyst system. The crude terephthalic acid is then purified, usually by hydrogenation, to give PTA. PTA reacts with mono-ethylene glycol in an esterification step that releases water, forming a low-molecular-weight prepolymer. This is polymerised further in the melt and often upgraded in the solid state to bottle-grade PET resin. Nearly all terephthalic acid goes into PET, with small volumes used for other polyesters.

Paso a paso

  1. Oxidise paraxylene with air in acetic acid
  2. Crystallise and filter crude terephthalic acid
  3. Purify by hydrogenation to PTA
  4. Esterify PTA with mono-ethylene glycol
  5. Melt polycondensation to PET prepolymer
  6. Solid-state upgrade for bottle grade
  7. Chip and ship

La química

Methyl groups on the ring are oxidised to carboxylic acid groups. The acid then forms ester bonds with the hydroxyl groups of ethylene glycol, giving the repeating terephthalate unit of PET.

Reacciones, dibujadas átomo a átomo

Paraxylene oxidationCc1ccc(C)cc1O=OO=OO=OOC(=O)c1ccc(C(=O)O)cc1OOC8H10 + 3 O2 -> C8H6O4 + 2 H2OAmoco process step.
Esterification with MEGOC(=O)c1ccc(C(=O)O)cc1OCCOOCCOC(=O)c1ccc(C(=O)O)cc1OC8H6O4 + C2H6O2 -> C10H10O5 + H2OFirst ester link of PET; repeating further builds the polymer.

Equipos principales

  • Titanium-lined oxidation reactor
  • Crystallisers
  • Hydrogenation reactor
  • Esterification vessel
  • Polycondensation reactors
  • Solid-state polymerisation unit

Seguridad

The bromide and acetic acid mix is highly corrosive, and hot air with organic vapour must be kept outside explosive limits.

En el Golfo

Gulf producers supply the chain mostly from the glycol and paraxylene ends rather than PET itself: MEG from Gulf ethylene (see the EO and MEG entry) and paraxylene from Iranian and regional aromatics units. Specific PTA or PET plant capacities are not stated for this entry.

Póngase a prueba

Pregunta 1 de 3 · Puntuación 0 · Racha 0

Which catalyst system is used in the Amoco PTA process?

Relacionado

Fuentes

Redactado con palabras propias de PST a partir de las fuentes anteriores. Fiabilidad de los datos: medium. Las plantas reales difieren en diseño y condiciones de operación.