Paraxylene is oxidised to purified terephthalic acid (PTA), which is reacted with mono-ethylene glycol to make PET for bottles, film and polyester fibre.

Carga de alimentação
Paraxylene, air, acetic acid, mono-ethylene glycol
Produz
Purified terephthalic acid (PTA), PET resin (bottle grade), Polyester fibre and film
Catalisador
Cobalt, manganese and bromide in acetic acid (oxidation)

Fluxo do processo

O que faz

In the Amoco process, paraxylene is oxidised with compressed air in acetic acid solvent, using a cobalt, manganese and bromide catalyst system. The crude terephthalic acid is then purified, usually by hydrogenation, to give PTA. PTA reacts with mono-ethylene glycol in an esterification step that releases water, forming a low-molecular-weight prepolymer. This is polymerised further in the melt and often upgraded in the solid state to bottle-grade PET resin. Nearly all terephthalic acid goes into PET, with small volumes used for other polyesters.

Passo a passo

  1. Oxidise paraxylene with air in acetic acid
  2. Crystallise and filter crude terephthalic acid
  3. Purify by hydrogenation to PTA
  4. Esterify PTA with mono-ethylene glycol
  5. Melt polycondensation to PET prepolymer
  6. Solid-state upgrade for bottle grade
  7. Chip and ship

A química

Methyl groups on the ring are oxidised to carboxylic acid groups. The acid then forms ester bonds with the hydroxyl groups of ethylene glycol, giving the repeating terephthalate unit of PET.

Reações, desenhadas átomo por átomo

Paraxylene oxidationCc1ccc(C)cc1O=OO=OO=OOC(=O)c1ccc(C(=O)O)cc1OOC8H10 + 3 O2 -> C8H6O4 + 2 H2OAmoco process step.
Esterification with MEGOC(=O)c1ccc(C(=O)O)cc1OCCOOCCOC(=O)c1ccc(C(=O)O)cc1OC8H6O4 + C2H6O2 -> C10H10O5 + H2OFirst ester link of PET; repeating further builds the polymer.

Equipamentos principais

  • Titanium-lined oxidation reactor
  • Crystallisers
  • Hydrogenation reactor
  • Esterification vessel
  • Polycondensation reactors
  • Solid-state polymerisation unit

Segurança

The bromide and acetic acid mix is highly corrosive, and hot air with organic vapour must be kept outside explosive limits.

No Golfo

Gulf producers supply the chain mostly from the glycol and paraxylene ends rather than PET itself: MEG from Gulf ethylene (see the EO and MEG entry) and paraxylene from Iranian and regional aromatics units. Specific PTA or PET plant capacities are not stated for this entry.

Teste seus conhecimentos

Pergunta 1 de 3 · Pontuação 0 · Sequência 0

Which catalyst system is used in the Amoco PTA process?

Relacionados

Fontes

Redigido com as palavras da própria PST a partir das fontes acima. Confiabilidade dos dados: medium. As plantas reais diferem em projeto e condições de operação.