跳至正文
登录申请报价

← 全部工艺

Delayed coking

Refinery process

Delayed coking heats vacuum residue in a furnace and lets it crack and turn to solid petroleum coke in large drums. It converts the worst heavy residue into lighter liquids and a solid by-product.

进料
Vacuum residue and other very heavy oils
产品
Petroleum coke, Coker gas, Coker naphtha, Coker gas oils
温度
About 480 to 505 at the furnace outlet
催化剂
None (thermal process)

工艺流程

功能

Residue from the vacuum unit is first fed to the bottom of a fractionator and then pumped through a furnace that raises it to about 480 to 505 degrees Celsius. Steam is injected in the tubes to limit coke forming in the furnace. The hot feed flows into one of a pair of coke drums where the cracking reactions continue and coke accumulates over 12 to 24 hours. Vapours leave overhead and are separated into gas, naphtha and gas oils. When a drum is full, flow switches to the second drum and the first is steamed, quenched with water and cut with high-pressure water jets to remove the coke. Coke is about 18 to 30 percent of the feed by weight.

分步说明

  1. Residue is preheated in the fractionator bottom
  2. A furnace heats the oil to about 480 to 505 C
  3. Steam is added to the tubes to slow fouling
  4. Hot feed enters a coke drum and cracks
  5. Vapour leaves overhead to the fractionator
  6. Coke builds in the drum over 12 to 24 hours
  7. Flow switches drums; the full drum is steamed, quenched and decoked with water jets

化学成分

Heat splits large carbon-carbon bonds to give smaller alkane and alkene fragments, while the hydrogen-poor remainder condenses into polyaromatic structures that harden into coke. The process rejects carbon as solid coke so the lighter liquids are richer in hydrogen.

逐个原子绘制的反应式

Thermal cracking of a long paraffinCCCCCCCCCCCCCCCCCCCCCCCCCCCCCCC=CCCCCCCCCC20H42 -> C10H22 + C10H20Light liquid fragments; the leftover carbon forms coke.

主要设备

  • Coker furnace
  • Paired coke drums
  • Main fractionator
  • Water cutting system
  • Coke handling and storage

安全

Opening a full drum can release hot coke and steam, and cutting operations have caused serious accidents. Hot residue and furnace coking are fire risks.

在海湾地区

The Ruwais Refinery opened a carbon black and delayed coker plant in 2018, per the facility history summarised on Wikipedia.

自我测验

第 1 题,共 3 题 · 得分 0 · 连对 0

About what furnace temperature?

相关

来源

由 PST 依据上述来源自行撰写。数据可信度:high。实际装置的设计和运行条件各有不同。