Sulphur recovery (Claus plus tail gas)
Refinery process
The Claus process turns hydrogen sulphide from amine units into elemental sulphur, which is sold. A tail gas unit then cleans up the small amount of sulphur compounds left.
- 进料
- Acid gas rich in H2S from amine units and sour water strippers
- 产品
- Liquid elemental sulphur, Treated tail gas (recycled or incinerated), Steam from waste heat boilers
- 温度
- Furnace above 850; catalytic stages about 315 to 330, 240 and 200
- 催化剂
- Activated alumina or titanium dioxide
工艺流程
功能
The acid gas from the amine regenerator is burned with a controlled amount of air in a reaction furnace so that about one third of the H2S becomes sulphur dioxide. The remainder of the H2S reacts with that SO2 to form elemental sulphur, and much of the sulphur is already formed in the furnace. The gas is cooled in a condenser to liquid sulphur, then reheated and passed through two or three catalytic stages, each followed by a condenser. A tail gas treatment unit removes most of what remains. Liquid sulphur is stored hot and sold or formed into solid granules.
分步说明
- Acid gas enters the reaction furnace with metered air
- One third of the H2S burns to SO2
- H2S and SO2 start reacting to elemental sulphur in the furnace
- A waste heat boiler and condenser cool the gas and remove liquid sulphur
- The gas is reheated and enters the first catalytic reactor
- Further condenser and reactor stages recover more sulphur
- Tail gas is treated and liquid sulphur is sent to a pit
化学成分
Part of the H2S is oxidised to sulphur dioxide, and then the Claus reaction between H2S and SO2 yields sulphur and water. The reaction is equilibrium-limited, which is why several stages are used. Cooling pushes the equilibrium toward sulphur. In practice the sulphur is a mix of S8 rings and smaller species, written simply as S in the equation.
逐个原子绘制的反应式
主要设备
- Reaction furnace
- Waste heat boiler
- Sulphur condensers
- Catalytic converters
- Tail gas treating unit
- Sulphur pit and degassing
安全
H2S and SO2 are toxic gases, and liquid sulphur can release H2S and cause pit fires. Lines must be kept hot to avoid solidification.
自我测验
What temperature does the Claus furnace exceed?
相关
来源
由 PST 依据上述来源自行撰写。数据可信度:high。实际装置的设计和运行条件各有不同。