Перейти к содержимому

← Все процессы

Hydrogen production (steam methane reforming)

Refinery process

A steam methane reformer converts natural gas and steam into hydrogen over a nickel catalyst. Refineries use it to supply hydrotreaters and hydrocrackers.

Сырьё
Natural gas or light hydrocarbons, steam
Производит
Hydrogen, Carbon dioxide, Export steam, PSA off-gas (fuel)
Температура
Outlet about 815 to 925
Давление
About 14 to 40
Катализатор
Nickel on alumina

Технологическая схема

Что делает

Natural gas is first desulphurised to protect the catalyst, then mixed with steam and sent through furnace tubes filled with nickel catalyst. The reaction is strongly endothermic, so the tubes are heated in a fired box. The gas leaves as synthesis gas containing hydrogen and carbon monoxide. A shift reactor then converts most of the carbon monoxide with steam to extra hydrogen and carbon dioxide. A pressure swing adsorption unit purifies the hydrogen, and the purge gas is burned as furnace fuel. Plants usually include a pre-reformer and waste heat recovery to raise steam.

Шаг за шагом

  1. Natural gas is desulphurised
  2. Steam is added at a steam-to-carbon ratio of about 2.5 to 3
  3. A pre-reformer converts heavier hydrocarbons to methane
  4. Reformer tubes in a fired furnace convert methane to syngas
  5. Waste heat boilers raise steam
  6. Shift reactors convert CO to more hydrogen
  7. PSA purifies the hydrogen

Химия

Methane reacts with steam over nickel to make carbon monoxide and hydrogen, absorbing about 206 kJ per mole. The water-gas shift reaction then converts carbon monoxide and water into carbon dioxide and more hydrogen. Sulphur poisons nickel, so it is removed first.

Реакции с отображением каждого атома

Steam methane reformingCO[C-]#[O+][H][H][H][H][H][H]CH4 + H2O -> CO + 3H2Strongly endothermic.
Water-gas shift[C-]#[O+]OO=C=O[H][H]CO + H2O -> CO2 + H2Mildly exothermic.

Основное оборудование

  • Desulphuriser
  • Pre-reformer
  • Reformer furnace with catalyst tubes
  • Shift converters
  • PSA unit
  • Waste heat boiler

Безопасность

Hydrogen is flammable across a wide range and carbon monoxide is toxic. Tube overheating can cause rupture.

Проверьте себя

Вопрос 1 из 3 · Счёт 0 · Серия 0

Typical SMR catalyst?

Связанное

Источники

Написано собственными словами PST по источникам выше. Достоверность данных: high. Реальные заводы различаются по конструкции и условиям работы.