Skip to content

Bitumen and solids

Polymer Modified Bitumen (PMB)

PMB is bitumen blended with polymers such as SBS to improve elasticity and temperature performance. It is used on heavy traffic roads and in roofing membranes.

← All productsAlso called: PMB, SBS modified bitumen, PG 76-22, Modified binder

  • Flash pointTypically above 220 C (varies by grade)
  • Density1000 to 1040 kg/m³
  • ViscositySoftening point at least 65 C for the PMB 45/80-65 grade
  • Sulphur1 to 6%
  • HazardUN3257 for hot bitumen shipped as an elevated temperature liquid, Class 9 (elevated temperature liquid, n.o.s., at or above 100 C and below its flash point)
Typical colour, laboratory glass
Laboratory glass sample of Polymer Modified Bitumen (PMB), in its typical colour
A sample of Polymer Modified Bitumen (PMB) in laboratory glass on a dark studio background, so the colour is easy to judge.
Reference photograph
How Polymer Modified Bitumen (PMB) is stored and moved in practice.

Image credits Laboratory glass samples are made from reference photos on Wikimedia Commons by Chemik10 (CC BY-SA 2.5) and a CC0 petroleum sample photo.

Polymer Modified Bitumen (PMB) is a solid at normal temperature, so there is no liquid to stir. Softening point at least 65 C for the PMB 45/80-65 grade

How it looks

Black

Where it is used

  • Heavy traffic roads
  • Airports
  • Bridge decks
  • Roofing membranes

Handling and safety

  • Store in insulated, heated tanks at 150 to 180 C; do not hold above 200 C for long because it ages and can foam if water is present. Avoid water contact (violent boiling). Sample with a heated sampler per ASTM D140 or EN 58 and test penetration, softening point and flash point. Trucks and ships need heating coils and loading arms with steam or thermal oil tracing. PMB can separate if stored hot too long; keep stirred.
  • Typically stored and moved at about 150 C (Wikipedia). Hot bitumen causes severe burns, and fumes can contain H2S and polycyclic aromatics. Check the local ADR/IMDG classification, which depends on the product and temperature.

Typical properties

Appearance
Black
Density at 15 °C
1000 to 1040 kg/m³
Flash point
Typically above 220 C (varies by grade)
Viscosity
Softening point at least 65 C for the PMB 45/80-65 grade
Pour point
Not applicable
Typical sulphur
1 to 6%

◉What it is

Polymer modified bitumen is conventional bitumen that has been blended with polymers. The most common is SBS (styrene-butadiene-styrene), which adds elasticity and resistance to rutting and cracking. Others are plastomers such as EVA and recycled rubber (Wikipedia mentions tyre rubber). PMB is graded by softening point, elastic recovery and penetration. It costs more than plain bitumen but extends pavement life.

⬡What it is made of

Bitumen plus 2 to 7% polymer; sometimes cross-linking agent such as sulphur.

⚛The chemistry

SBS has hard polystyrene end blocks and soft polybutadiene mid blocks. In bitumen the blocks form a network that gives rubber-like elasticity.

⚙How it is made

Base bitumen is mixed with polymer in high shear mills at 170 to 190 C, then held for swelling.

▶How it works

The polymer network lets the binder stretch and recover, so pavement resists rutting in summer and cracking in winter.

▣Storage, loading and inspection

Store in insulated, heated tanks at 150 to 180 C; do not hold above 200 C for long because it ages and can foam if water is present. Avoid water contact (violent boiling). Sample with a heated sampler per ASTM D140 or EN 58 and test penetration, softening point and flash point. Trucks and ships need heating coils and loading arms with steam or thermal oil tracing. PMB can separate if stored hot too long; keep stirred.

★Why it matters in the Gulf

PMB is relevant for Gulf highways and airports where summer pavement temperatures are very high. Regional plant details are not stated.

Key molecules

Standards and specifications

EN 14023European framework specification for polymer modified bitumens.
AASHTO M 320 and M 332Performance-graded binder specifications, M 332 using the multiple stress creep recovery test.
ASTM D6373Performance-graded asphalt binder.

Hazards

UN3257 for hot bitumen shipped as an elevated temperature liquidClass Class 9 (elevated temperature liquid, n.o.s., at or above 100 C and below its flash point)

Typically stored and moved at about 150 C (Wikipedia). Hot bitumen causes severe burns, and fumes can contain H2S and polycyclic aromatics. Check the local ADR/IMDG classification, which depends on the product and temperature.

How it is traded

Units

Metric tonnes

Benchmarks

Contract price; premium over 60/70

Typical cargo

Tank truck, ISO tank, drums

Incoterms

DAP, FCA, FOB

Notes

Priced at a premium over plain bitumen; the premium varies by market.

Refineries that make it: our suggestions

73 listed refineries make this product, 22 of them in the Gulf, Iran and Iraq. We rank Gulf plants first, then operating plants, then by capacity.

See all 73 on the map

Terminals that handle it

Did you know

💡 SBS is the polymer most often used to modify bitumen.

💡 Polymer modification raises elasticity and resistance to rutting.

Test yourself on Polymer Modified Bitumen (PMB)

Question 1 of 3 · Score 0 · Streak 0

Common polymer in PMB?

More in this group

Sources

Written in PST's own words from the sources above. Confidence in the data: medium. Typical values vary by origin and contract, so always read the specification in your own contract.